…after an extended period of PETG, and I have to say I think my favorite part is after the print ends and the bed starts to cool off and the snap/crackle/pop of the piece coming off on it’s own. Such a pleasant ASMR experience.

Highly recommend…

    • B0rax
      link
      fedilink
      English
      arrow-up
      2
      ·
      7 hours ago

      Then your ambient air while printing is too cold. You need a chamber with >40°C